Refer to tables A-20, A-21, A-22, A-24c
a) for UNS G10200 hot rolled steel, Sut = 380 MPa, Syt = 210 MPa
b) for SAE 1050 cold drawn steel, Sut = 690 MPa, Syt = 580 MPa
c) for AISI 1141 steel quenched and tempered, Sut = 896 MPa, Syt = 765 MPa
d) for 2024-T4 aluminium alloy, Sut = 446 MPa, Syt = 296 MPa
e) for Ti-6Al-4V annealed titanium alloy, Sut = 900 MPa, Syt = 830 MPa
Here, Sut= Tensile strength and Syt= Yield Strength. Units of MPa can also be converted to kpsi if needed using 1 MPa = 0.145 ksi